Hi,

I'm after some advice regarding the replastering of damp areas due to hygroscopic salts.

Background:

About a year ago my girlfriend's house (Victorian - 1900ish) started showing damp patches on the internal walls. We contacted the council, who (after a number of builder's visiting us) advised us that we had raising damp in ALL of our walls and the walls needed to be injected and replastered.

A few weeks ago, we decided not to wait for the council any more (we were applying for a grant to get the job done) and got a damp proof specialist in. He walked in the front door, smiled and told us instantly that we didn't have rising damp. He examined the walls and told us that damp proofing had already been done on the walls (not by him) and it was the hygroscopic salts penetrating the "new" plaster which was causing the damp.

He advised us the best thing to do would be to remove the plaster at the damp places and re-plaster with a sand/cement/waterproofer mix. He did not charge for the visit!

Advice needed:

Ok, due to our relief (the cost wasn't going to be thousands!) and our anger (the council allowing contractors to rip them, and us, off) I never actually asked some simple questions: Simply put:

1. What type of sand? (Building sand, sharp sand, etc?)
2. Should we allow the wall to dry once the old plaster is removed before replastering?
3. How long do we need to wait before putting paper on the wall again? (he said we could paint after a month)

Also, any other advice would be helpful, thanks.
 
Sponsored Links
Noseall, thankyou I will look into that further.

After doing some research I have come up with the following process:

1. Preperation
Remove plaster up to a height 30cm (1ft) above visible dampness.
Rake out mortar joints to 12mm (1/2") deep.

2. First coat
Mix 3 parts Grade 'M' (sharp, loam free) sand to one part cement with waterproofer (at suggested mix) using no more than 1litre of water for 6.25kg of dry mix.
Compact into raked out joints and render to a thickness of 12mm (1/2").
Key render.

3. Second coat
Repeat mix for first coat excluding waterproofer.
Render to an additional thickness of 12mm (1/2").
Key Render.

4. Third coat
Use a porous finishing plaster to finish the surface.

Between each coat the render should be allowed to set a bit.

Does this sound good, or am I missing something important? (ie the sbr slurry mix)
 

DIYnot Local

Staff member

If you need to find a tradesperson to get your job done, please try our local search below, or if you are doing it yourself you can find suppliers local to you.

Select the supplier or trade you require, enter your location to begin your search.


Are you a trade or supplier? You can create your listing free at DIYnot Local

 
Sponsored Links
Back
Top