908 should be mixed with warm/tepid water when used as a primer. Cold water will congeal the dpm. It will always have a tacky finish unfortunately in the past we have had to use boards to do further coats.
 
Sponsored Links
The warm water makes sense, would help if it said on the instructions.

I put a 2nd coat around the edges and up the walls then put a sheet dpm over the whole thing in the end.

I don't think it's a good idea to use this as dpm on floors just creates problems, a sheet is a far more practical option.
 