My mate has had a new pumped concete screed laid in his whole ground floor. They have UFH.
He let the place dry out for 11 days and then slowly introduced heat.
He has had quite a bit of cracking especially around the doors.
He is planning on laying a new very thin cement screed and laying some mesh product into it.
I said this was a bit OTT and thought i would ask opinions on here what he should do.
I was wondering if the BAL stopgap product would be all he needs to lay down:
http://www.directflooringcentre.co....utM9DYuGi1WpW0PuDU1G7H374gLi7FFBoCV1UQAvD_BwE
Advise appreciated
He let the place dry out for 11 days and then slowly introduced heat.
He has had quite a bit of cracking especially around the doors.
He is planning on laying a new very thin cement screed and laying some mesh product into it.
I said this was a bit OTT and thought i would ask opinions on here what he should do.
I was wondering if the BAL stopgap product would be all he needs to lay down:
http://www.directflooringcentre.co....utM9DYuGi1WpW0PuDU1G7H374gLi7FFBoCV1UQAvD_BwE
Advise appreciated